HalFoam™ – Fibre free ceramic foam

HalFoam™ is the brand for fibre free ceramic foam materials made of aluminium oxide or silicon dioxide. Unlike ceramic fibre boards our HalFoam™ products do not contain any fibre components. HalFoam™ is fully EHS compliant. There are no harmful dusts created during machining or handling of the material.

Our environmentally friendly foaming process allows for a very high and homogeneous porosity. 

HalFoam™ is characterised by the following properties:

  • Low thermal conductivity
  • Excellent refractoriness
  • High material-specific corrosion resistance
  • Very good thermal shock properties
  • High mechanical strength
  • Low relative density (low specific gravity)