MgO Spinel Kiln Furniture

We now provide a wide range of kiln furniture including setting plates, beams, supports etc and crucibles made from our specialist magnesium oxide (MgO) Spinel material.

Our MgO Spinel can be used for products up to a temperature range of 1700oC and exhibits superior corrosion resistance particularly against alkalis and earth alkalis.

The properties of this material make it particularly good for products used within metal melting (non-iron) and has shown to perform well in the melting of light metals containing aggressive slags.

This material offers a wide range of benefits for our products including:

  • High thermal conductivity of 12-14W/mK
  • Excellent thermal shock reistance
  • High electrical resistivity

which makes this suitable for a wide range of applications.

Our qualified engineers work closely with our customers to produce customised crucibles and kiln furniture to a high quality standard.

To find out how we can help you with your project, contact us today.