Collision Cells

We manufacture a range of collision cells which are manufactured to customer specification.

Our mass spectrometer collision cells are predominately made from 97.5% alumina selected for its thermal stability and electrical properties. Alumina can be precision-machined to tight tolerances making it ideal for producing high quality parts to customer specifications. Ceramic and metal components can be brazed together or metalized for conductivity.

We can help you to develop and manufacture complex collision cells for mass spectrometer applications. With our extensive engineering expertise, we can offer cost efficient configurations incorporating various materials, machining techniques and coating technologies in a single part.

For more information on the use of our alumina collision cells in your mass spectrometer