Plates are normally cut from an option of three alternative standard sizes, i.e. Iateral dimensions of 40 x 20mm, 50 x 50mm, 89 x 42mm. Still larger sizes up to 150mm lengths can be cut from discs.

Thicknesses range from 0.2 to 15mm but not in every combination in every material.

 

Piezoelectric Flat Plate Standard piezoelectric plate side view

 

Freq F Thickness T 5 x 5 8 x 8 10 x 10 15 x 15 20 x 20 25 x 25 40 x 20 50 x 50 89 x 42
MHz mm                  
0.13 15                  
0.20 10
0.25 8
0.30 6
0.40 5
0.50 4
0.75 3
1.0 2
1.5 1.5  
2.0 1  
2.25 0.9    
2.5 0.8    
3.0 0.6    
4.0 0.5    
5.0 0.4      
10 0.2        