Injection Moulding

Stage 1
Ceramic powders and organics are added to a special mixing device and intimately mixed together

Stage 2
The resultant mix is granulated and fed into an injection moulding machine

Stage 3
A ‘ram’ forces the ceramic into a ‘heated zone’ that liquifies the binder and allows the ceramic to flow under pressure into a mould

Stage 4
The mould and the formed ceramic component is cooled quickly to form a solid

Stage 5
The mould is split and the solid ceramic component is ejected

About us

Morgan Technical Ceramics is a division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.