Stage 1
Ceramic components, after debinding, are placed in a high temperature kiln for densification

Stage 2
The kiln is heated up evenly and at a certain temperature, densification will occur when porosity is reduced or eliminated and grains within the ceramic will grow

Stage 3
The kiln will cycle through a predefined temperature – time profile and once back at ambient temperature, the ceramic components can be removed

About us

Morgan Technical Ceramics is a business of the Morgan Ceramics Division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

 

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.