Piezo Ceramics & Assemblies

Piezoceramics have the special ability to turn electrical energy into mechanical force or vice versa. This has led them to be used for sensor and transducer applications in many demanding conditions. The alteration in shape is a natural phase change so the material is left undamaged.

Morgan Electro Ceramics offer a wide range of Lead Zirconate Titanate piezo-ceramics. Each type is tailored to enhance specific properties and to the requirements of particular applications.

Typical characteristics include:

  • Produces very large forces
  • Fast expansion
  • No lubricants or abrasion
  • Clean room and vacuum safe
  • Extremely fine motor control

Typical applications include:

  • Power ultrasonics
  • Flow and level measurement
  • Gyroscopes
  • Accelerometers

Piezo Ceramics & Assemblies AEROSPACE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Fuel Level Sensors
  • Gyroscopes
  • Vibration Sensors

Piezo Ceramics & Assemblies AUTOMOTIVE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Parking Sensors
  • Knock Sensors
  • Fuel Injection
  • Fuel Level Sensors
  • Piezo Motors
  • Crash Sensors
  • Wheel Balancing
  • Noise Cancellation

Piezo Ceramics & Assemblies ELECTRONICS

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Transformers
  • Hard Disc Drives
  • Suspension Arms
  • Surface Testing
  • Anti Vibration
  • Ink Jet Printing

Piezo Ceramics & Assemblies INDUSTRIAL EQUIPMENT

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Ultrasonic Welding
  • Level Sensors
  • Flow Sensors

Piezo Ceramics & Assemblies MEDICAL

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Blood Flow
  • Foetal Heart Monitors
  • Medical Imaging
  • Nebulisation
  • Catheters
  • Pacemakers
  • Cataract Removal
  • Ultrasonic Scalpels
  • DNA Testing

Piezo Ceramics & Assemblies POWER DISTRIBUTION

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Power ultrasonics
  • Impedance Analyser
  • Flow and level measurement
  • Gyroscopes
  • Accelerometers

Piezo Ceramics & Assemblies PROCESS CONTROL & MONITORING

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Ultrasonic Welding
  • Level Sensors
  • Flow Sensors

Piezo Ceramics & Assemblies SECURITY & DEFENCE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Dipping Sonar
  • Sonar Buoys
  • Submarine & Surface Sonar
  • Torpedo Guidance

Piezo Ceramics & Assemblies SEMICONDUCTOR PROCESSING

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Megasonic Cleaning
  • Micropositioning actuators

 

Contact Technical Materials
About us

Morgan Technical Ceramics is a business of the Morgan Ceramics Division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

 

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.