Zirconia (TZP)

Zirconia (TZP) offers chemical and corrosion resistance to temperatures well above the melting point of Alumina.

In its pure form crystal structure changes limit mechanical applications, however stabilised Zirconias produced by addition of Calcium, Magnesium or Ytrium Oxides can produce very high strength, hardness and particularly toughness. In addition the material has low thermal conductivity and is an ionic conductor above 600ºC. This has lead to applications in oxygen sensors and high temperature fuel cells.

 

Typical Zirconia characteristics include:

  • High temperature capability up to 2400ºC
  • High density
  • High strength and fracture toughness
  • High hardness and wear resistance
  • Low thermal conductivity (20% that of Alumina)
  • Good chemical resistance
  • Ionic conductivity

Typical Zirconia applications include:

  • Precision ball valve (balls and seats) Pump seals, valves and impellors
  • High density grinding media
  • Oxygen sensors
  • Threadguides
  • Fuel cell membranes
  • Cutting blades
  • Radio frequency heating susceptors
  • Medical prostheses
  • Metrology components
     

 

Contact Technical Materials
About us

Morgan Technical Ceramics is a business of the Morgan Ceramics Division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.