Steatite

Steatite is a Magnesium Silicate material. It is formed using standard ceramic processing methods and can readily be machined or net shape sintered into a variety of forms.

The material is lower in cost than Alumina but offers reduced mechanical properties. However Steatite has very good electrical resistance properties, which are retained at high temperatures, along with moderate mechanical strength and temperature resistance. It has been used in electrical insulation for many years in both large-scale electrical systems and electronic and domestic appliances.

Typical Steatite characteristics include:

  • Good to excellent electrical properties
  • High resistivity
  • Very low dielectric loss factor
  • Moderate strength
  • Low density

Typical Steatite applications include:

  • Regulator bases
  • Switches and plug parts
  • Sockets
  • Bases for halogen lamps
  • Heating Element Holders
  • Stand-Off Insulators
  • Washers and Bushings
     

 

Contact Technical Materials
About us

Morgan Technical Ceramics is a division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.