Aluminium Nitride

Morgan Technical Ceramics utilise the properties of Aluminium Nitride to find effective solutions in challenging applications. The high thermal conductivity and excellent electrical insulation makes Aluminium Nitride suitable for a range of extreme environments.

Aluminium Nitride is a high performance material particularly suited to demanding electrical applications. At Morgan Technical Ceramics we combine expansive technical understanding with a commitment to working with customers, ensuring that our material solutions meet exacting specifications whilst providing exceptional performance.

Aluminium Nitride can be produced by dry press and sinter or by hot pressing with appropriate sintering aids, the result of these processes is a material that is stable at high temperatures in a range of inert environments including hydrogen and carbon dioxide atmospheres. Aluminium Nitride is principally used in the electronics area, particularly when heat removal is an important function.

Aluminium Nitride properties also make it particularly useful in the creation of corrosion resistant products. At Morgan Technical Ceramics our unique approach to developing and manufacturing means that our engineers collaborate with customers to ensure that corrosion resistant products or components consistently satisfy customer requirements.

Typical Aluminium Nitride characteristics include:

  • Very good thermal conductivity
  • Thermal expansion coefficient similar to that of Silicon
  • Good dielectric properties
  • Good corrosion resistance
  • Stability in semiconductor processing atmospheres

Typical Aluminium Nitride applications include:

  • Heat sinks
  • Electronic substrates
  • IC packages
  • Power transistor bases
  • Microwave device packages

Contact us now to discover how we could utilise Aluminium Nitride in your market specific applications.

Contact Technical Materials
About us

Morgan Technical Ceramics is a business of the Morgan Ceramics Division of The Morgan Crucible Company plc. We design and manufacture products for demanding applications in a variety of markets using a comprehensive range of advanced ceramic, glass, precious metal, piezoelectric and dielectric materials Read company details here.

The Morgan Crucible Company plc is registered in England
Registered office at Quadrant, 55-57 High Street, Windsor, Berkshire, SL4 1LP. Company number: 286773.