Ion Beam & RF Plasma Depositions

Stage 1
Products to be coated are placed in the chamber

Stage 2
The chamber is heated, evacuated and components are rotated

Stage 3
At the appropriate temperature and pressure, gases are fed into the chamber and coatings are deposited onto components

Stage 4
After an appropriate thickness has been deposited, gases stop flowing and the chamber and components are cooled to ambient temperature

Please use our contact page if you require any further information.


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China