Chemical Vapour Deposition
(CVD)
Stage 1
Moulds are incorporated into the kiln where they are coated and shape the CVD material
Stage 2
The chamber is sealed and evacuated and heated up
Stage 3
At the correct temperature, a mixture of gases are fed into the chamber and react and deposit onto the surface of the ‘moulds’
Stage 4
The gases continue to be fed to build up the correct thickness of material
Stage 5
Gases finally stop flowing and the chamber is cooled to ambient temperature
Please
use our contact page if you require any further
information.
|
Key
Markets | Manufacturing
Sites | New
Technologies | Materials
| Glossary
of Terms | Quality
/ Environment | News
& Information | Contact
Us | Home Page
| Sitemap
Morgan
Technical Ceramics is a Global Business Unit of the Morgan
Crucible Company plc.
It comprises Morgan
Advanced Ceramics and Morgan
Electro Ceramics
Sales Offices/Customer
Service:
Europe:
Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg,
Germany
UK
and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc
DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS,
Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul,
Turkey
USA:
Morgan Technical Ceramics, 232 Forbes Road,
Bedford,
Ohio 44146-5418, USA
Asia:
Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818,
China |
|