Zirconia (TZP)

Zirconia (TZP) offers chemical and corrosion resistance to temperatures well above the melting point of Alumina. In its pure form crystal structure changes limit mechanical applications, however stabilised Zirconias produced by addition of Calcium, Magnesium or Ytrium Oxides can produce very high strength, hardness and particularly toughness. In addition the material has low thermal conductivity and is an ionic conductor above 600ºC. This has lead to applications in oxygen sensors and high temperature fuel cells.

Typical characteristics include:

  • High temperature capability up to 2400ºC
  • High density
  • High strength and fracture toughness
  • High hardness and wear resistance
  • Low thermal conductivity (20% that of Alumina)
  • Good chemical resistance
  • Ionic conductivity

Typical applications include:

  • Precision ball valve (balls and seats) Pump seals, valves and impellors 
  • High density grinding media 
  • Oxygen sensors 
  • Threadguides 
  • Fuel cell membranes
  • Cutting blades 
  • Radio frequency heating susceptors
  • Medical prostheses
  • Metrology components 
   
Advanced Ceramics
Alumina
Aluminium Nitride
Aluminium Silicate
CD (Charge Dissipative) Alumina
Cordierite
CVD Silicon Carbide
Fused Silica
MACOR (Machineable Glass Ceramic)
Magnesium Oxide
Pyrolytic Boron Nitride (PBN)
Silicon Carbide (SiC)
Silicon Nitride (Si3N4)
Steatite
Titania
Zirconia (TZP)
Zirconia Toughened Alumina (ZTA)
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China