Advanced Ceramics  

Titania

Whilst Titania (Titanium Dioxide) is used in large quantities in powder form, bulk sintered material has limited mechanical applications, due to its relatively low fracture toughness compared to Alumina. This material is tan in colour, and has been used to produce threadguides where the relatively ‘soft’ ceramic is easier to polish and gives a kinder surface to more sensitive chemical fibres. In addition the material can be produced in a reduced form, black in colour, that is electrically conductive for threadguide applications where static electricity is a problem 

Typical characteristics include:

  • Low friction
  • High thermal conductivity
  • Corrosion resistant
  • Moderate strength
  • High dielectric properties in pure form
  • Electrical conductivity in reduced form

Typical applications include:

  • Threadguides
   
Advanced Ceramics
Alumina
Aluminium Nitride
Aluminium Silicate
CD (Charge Dissipative) Alumina
Cordierite
CVD Silicon Carbide
Fused Silica
MACOR (Machineable Glass Ceramic)
Magnesium Oxide
Pyrolytic Boron Nitride (PBN)
Silicon Carbide (SiC)
Silicon Nitride (Si3N4)
Steatite
Titania
Zirconia (TZP)
Zirconia Toughened Alumina (ZTA)
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China