Advanced Ceramics
Pyrolytic
Boron Nitride
Pyrolytic Boron Nitride (PBN) is a white solid material that is non-porous, and non-toxic. Whilst Boron Nitride can be formed by pressing/sintering methods, the high purity pyrolytic material is formed by a vapour deposition process. The material is highly anisotropic in its electrical and mechanical properties, and very resistant to thermal shock. PBN is also a very good electrical insulator and has very high thermal conductivity. The material is stable in inert and reducing atmospheres up to 2800°C, and in oxidizing atmospheres to 850°C.
Typical characteristics include:
- High thermal conductivity
- Low thermal expansion
- Excellent thermal shock resistance
- High electrical resistance
- Low dielectric constant and loss tangent
- Good chemical resistance
Typical applications include:
- Electrical insulation
- Heating elements
- Crucibles & boats for crystal growth of semiconductor materials
- Semiconductor wafer processing equipment
|
|
Key
Markets | Manufacturing
Sites | New
Technologies | Materials
| Glossary
of Terms | Quality
/ Environment | News
& Information | Contact
Us | Home Page
| Sitemap
Morgan
Technical Ceramics is a Global Business Unit of the Morgan
Crucible Company plc.
It comprises Morgan
Advanced Ceramics and Morgan
Electro Ceramics
Sales Offices/Customer
Service:
Europe:
Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg,
Germany
UK
and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc
DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS,
Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul,
Turkey
USA:
Morgan Technical Ceramics, 232 Forbes Road,
Bedford,
Ohio 44146-5418, USA
Asia:
Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818,
China |
|