Piezo Ceramics & Assemblies

Piezoceramics have the special ability to turn electrical energy into mechanical force or vice versa. This has led them to be used for sensor and transducer applications in many demanding conditions. The alteration in shape is a natural phase change so the material is left undamaged.

Morgan Electro Ceramics offer a wide range of Lead Zirconate Titanate piezo-ceramics. Each type is tailored to enhance specific properties and to the requirements of particular applications. 

Typical characteristics include:

  • Produces very large forces
  • Fast expansion
  • No lubricants or abrasion
  • Clean room and vacuum safe
  • Extremely fine motor control

Typical applications include:

  • Power ultrasonics
  • Impedance Analyser
  • Flow and level measurement
  • Gyroscopes
  • Accelerometers

Piezo Ceramics & Assemblies AEROSPACE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Fuel Level Sensors
  • Gyroscopes
  • Vibration Sensors

Piezo Ceramics & Assemblies AUTOMOTIVE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Parking Sensors
  • Knock Sensors
  • Fuel Injection
  • Fuel Level Sensors
  • Piezo Motors
  • Crash Sensors
  • Wheel Balancing
  • Noise Cancellation

Piezo Ceramics & Assemblies ELECTRONICS

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Transformers
  • Hard Disc Drives
  • Suspension Arms
  • Surface Testing
  • Anti Vibration
  • Ink Jet Printing

Piezo Ceramics & Assemblies INDUSTRIAL EQUIPMENT

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Ultrasonic Welding
  • Level Sensors
  • Flow Sensors

Piezo Ceramics & Assemblies MEDICAL

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Blood Flow
  • Foetal Heart Monitors
  • Medical Imaging
  • Nebulisation
  • Catheters
  • Pacemakers
  • Cataract Removal
  • Ultrasonic Scalpels
  • DNA Testing

Piezo Ceramics & Assemblies POWER DISTRIBUTION

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Power ultrasonics
  • Impedance Analyser
  • Flow and level measurement
  • Gyroscopes
  • Accelerometers

Piezo Ceramics & Assemblies PROCESS CONTROL & MONITORING

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Ultrasonic Welding
  • Level Sensors
  • Flow Sensors

Piezo Ceramics & Assemblies SECURITY & DEFENCE

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Dipping Sonar
  • Sonar Buoys
  • Submarine & Surface Sonar
  • Torpedo Guidance

Piezo Ceramics & Assemblies SEMICONDUCTOR PROCESSING

Typical characteristics include:

  • Produce large forces at high speeds
  • Produce large displacements at high speeds
  • Monitor and detect vibrations
  • Can withstand a range of operating temperatures and environmental conditions
  • Can transmit and receive ultrasonic signals

Typical applications include:

  • Ultrasonic Cleaning
  • Megasonic Cleaning
  • Micropositioning actuators
   
Advanced Ceramics
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China