Cordierite

Cordierite is a Magnesium Alumina Silicate material. Its most important feature is that it has a very low coefficient of thermal expansion and excellent resistance to thermal shock. It is also similar to Steatite in that it is relatively low cost, has good electrical insulation properties, has moderate mechanical properties and temperature resistance, and can readily be formed in a variety of shapes. In particular it can be made in high volume through cost-effective extrusion or dry-pressing methods.

Typical characteristics include:

  • Low thermal expansion coefficient

  • High resistance to thermal shock

  • Volume resistivity

  • Low dielectric loss factor

  • Moderate strength

  • Low density

Typical applications include:

  • Electrical insulators 

  • Feed-thru insulators 

  • High performance resistors 

  • Special furnace shapes

  • Heating element supports 

  • Exhaust catalyst supports

  • Burner tubes

   
Advanced Ceramics
Alumina
Aluminium Nitride
Aluminium Silicate
CD (Charge Dissipative) Alumina
Cordierite
CVD Silicon Carbide
Fused Silica
MACOR (Machineable Glass Ceramic)
Magnesium Oxide
Pyrolytic Boron Nitride (PBN)
Silicon Carbide (SiC)
Silicon Nitride (Si3N4)
Steatite
Titania
Zirconia (TZP)
Zirconia Toughened Alumina (ZTA)
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China