Aluminium Silicate

This material, manufactured under the trade name Sillimantin 60 NG, is a porous Alumina Silicate which, due to its structure, remains porous even after high temperature firing. 

Sillimantin 60 NG is most frequently used in furnace construction and for rollers used in Roller Hearth Furnaces, primarily within zones operating between 1100°C - 1300°C, where alternative materials often fail.

Typical characteristics include:

  • Excellent High Temperature capability

  • Exceptional thermal shock resistance

  • Low and very stable thermal expansion coefficient

  • Hard and Durable, with excellent resistance to abrasion and chemical attack

  • Can be precision formed into complex shapes that are not easily achieved with other materials

Typical applications include:

  • Thermal Insulation components

  • Dicing support plates for wafer slicing

  • Furnace fixtures for glass sealing

  • Welding Nozzles

  • Kiln Furniture

  • Kiln structural components

   
Advanced Ceramics
Alumina
Aluminium Nitride
Aluminium Silicate
CD (Charge Dissipative) Alumina
Cordierite
CVD Silicon Carbide
Fused Silica
MACOR (Machineable Glass Ceramic)
Magnesium Oxide
Pyrolytic Boron Nitride (PBN)
Silicon Carbide (SiC)
Silicon Nitride (Si3N4)
Steatite
Titania
Zirconia (TZP)
Zirconia Toughened Alumina (ZTA)
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China