Alumina

Aluminium Oxide, Al2O3 is a major engineering material. It offers a combination of good mechanical properties and electrical properties leading to a wide range of applications. Alumina can be produced in a range of purities with additives designed to enhance properties. A wide variety of ceramic processing methods can be applied including machining or net shape forming to produce a wide variety of sizes and shapes of component. In addition it can be readily joined to metals or other ceramics using metallising and brazing techniques.

Alumina based ceramics are by far the largest range of advanced ceramics made by Morgan Technical Ceramics. Due to the important combination of properties, we have thoroughly researched the behaviour and characteristics of our Alumina products to give you the best possible component. 

Typical characteristics include:

  • Good strength and stiffness
  • Good hardness and wear resistance
  • Good corrosion resistance
  • Good thermal stability
  • Excellent dielectric properties (from DC to GHz frequencies)
  • Low dielectric constant
  • Low loss tangent

Typical applications include:

  • Seal rings
  • Medical prostheses
  • Laser tubes
  • Electronic substrates
  • Ballistic armour
  • Thermocouple tubes
  • Electrical insulators
  • Grinding media
  • Threadguides
  • Wear components
   
Advanced Ceramics
Alumina
Aluminium Nitride
Aluminium Silicate
CD (Charge Dissipative) Alumina
Cordierite
CVD Silicon Carbide
Fused Silica
MACOR (Machineable Glass Ceramic)
Magnesium Oxide
Pyrolytic Boron Nitride (PBN)
Silicon Carbide (SiC)
Silicon Nitride (Si3N4)
Steatite
Titania
Zirconia (TZP)
Zirconia Toughened Alumina (ZTA)
Electro Ceramics
Braze Alloys
Metal Injection Moulding
Coatings
Glass Products

 


Key Markets | Manufacturing Sites | New Technologies | Materials | Glossary of Terms | Quality / Environment | News & Information | Contact Us | Home Page | Sitemap

Morgan Technical Ceramics is a Global Business Unit of the Morgan Crucible Company plc.
It comprises Morgan Advanced Ceramics and Morgan Electro Ceramics

Sales Offices/Customer Service:
Europe: Morgan Technical Ceramics, Teplitzerstr.27, D-84478 Waldkraiburg, Germany
UK and Eire: Morgan Technical Ceramics, Bewdley Road, Stourport, Worc DY13 8QR, England
Middle East: Morgan Karbon Grafit Sanayi AS, Ikitelli OSB, Eskoop Sanayi Sitesi, B2 Blok, N.156, 34670 Ikitelli, Istanbul, Turkey
USA: Morgan Technical Ceramics, 232 Forbes Road, Bedford, Ohio 44146-5418, USA 
Asia: Morgan Technical Ceramics, 158 Jiajian Road, Jiading, Shanghai 201818, China