Glass Preforms

Glass Preforms from Morgan Advanced Materials are precision engineered and produced in high volumes for a cost effective solution, whatever your application and industry.

Our stringent manufacturing batch controls can be relied on to ensure that your components will perform to specification, even when produced in high volumes.

We offer more than 300 compositions of hermetic glass to metal seals. We have the capability to manufacture compression seals, alumina stepped seals and customised formulations, and products such as relays, fuses and fibre optic connectors.

We are committed to research and development and continue to improve the range of expansion coefficients available currently thermal expansions ranging from 32 to 130 x107 in/in/⁰C.