 | |  | Morgan Advanced Ceramics Inc - Approved Corning Distributors of MACOR
Please be aware that due to technical issues, ordering two or more different items from a catalogue page causes an error. If you need two different items from a single page, add them to the cart as separate items. Quantities of a single item are not affected.
Ordering your standard size MACOR products is now a whole lot quicker and easier. New and current customers can Apply for a Customer Account TODAY and make the order process even faster. |
| Making A Purchase Making a purchase could not be easier. Just browse our store, and add any items that you wish to buy into the shopping cart. After you have finished your selection, click on 'Checkout' and you will be asked for a few details that we need to be able to complete the order. If you are shopping from North America or anywhere else, place your order and your credit card company will convert the transaction to US Dollars or your own currency. |
| Credit Card Security When the order is placed at our website, credit card numbers are encrypted using 128 bit encryption. They are only decrypted after they reach our computer. They are not held in clear text on any web site. |
| Reaching Us If you need to reach us, please email us using the link on the store page, alternatively, you can call on (973) 227-8877 (International +001 (973) 227-8877) or fax us on (973) 227-7135 or write to us at 26 Madison Road Fairfield NJ 07004 United States. |
| Non Standard MACOR Shapes Inquiries for non standard MACOR sizes and shapes can be made using this email link. Drawings can be attached to your email or send using the FAX number above.
If it is a simple shape that is not found on our standard list, please list the details below in the body of your email:
>Rod, sheet or bar
>Sizes required
>Tolerances required
>Quantity required |
| Contact Us Customers can also use the contact form for general inquiries or to request further information. |
| About MACOR® Machinable Glass Ceramic > Is MACHINABLE with ordinary metal working tools > Allows FAST TURNAROUND. No post firing required > Holds TIGHT TOLERANCES, up to .0005" > Withstands HIGH TEMPERATURES, up to 1000oC (no load) > Is CLEAN, no outgasing and zero porosity.
With MACOR Machinable Glass Ceramic (MGC), fabrication is fast because it can be machined into complicated shapes and precision parts with ordinary metal working tools, quickly and inexpensively, and it requires no post firing after machining. That means no frustrating delays, no expensive hardware, no post fabrication shrinkage, and no costly diamond tools to meet specifications.
Properties
MACOR® Machinable Glass Ceramic has a continuous use temperature of 800oC and a peak temperature of 1000oC. Its coefficient of thermal expansion readily matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and unlike ductile materials, won't deform. It is an excellent insulator at high voltages, various frequencies, and high temperatures. When properly baked out, it won't outgas in vacuum environments.
Further details can be found in our MACOR Properties and Applications Information.
|